Metals and metal oxides surfaces

Vanadium films
Mode:Semicontact mode
SPM Model:Solver P47-PRO
Scan size:2x2 µm
Res. frequency:270 kHz
Source MDT-file:download (130.42 Kb)

Film of vanadium oxide on glass surface.
Vanadium sputtered on glass with the subsequent oxidation in natural conditions. Annealing of the sample was carried out at 500 îÑ during 10 min in dry oxygen.

Image courtesy of Gusev E.Yu., Taganrog State University Of Radioengineering.
The sample was kindly given by Dzhuplin V.N., Ageev O.A., Taganrog State University Of Radioengineering.